Abstract: A method including reducing a particle size of lignin particles to an
average particle size less than 40 nanometers; after reducing the
particle size, combining the lignin particles with a polymeric material;
and forming a structure of the combination. A method including exposing
lignin to a diazonium precursor including a functional group; modifying
the lignin by introducing the functional group to the lignin; and
combining the modified lignin with a polymeric material to form a
composite. An apparatus including a composite of a polymer and lignin
wherein the lignin has an average particle size less than 100
micrometers. |
Filed: 8/29/2012 |
Application Number: 13/597928 |
This invention was made with Government support under Contract No. DE-NA0003525 awarded by the United States Department of Energy/National Nuclear Security Administration. The Government has certain rights in the invention. |
Attribution for Derwent World Patents Index Records published on Sandia ® echo date('Y'); ?> Clarivate. All rights reserved. Republication or redistribution of Clarivate content, including by framing or similar means, is prohibited without the prior written consent of Clarivate. Clarivate and its logo, as well as all other trademarks used herein are trademarks of their respective owners and used under license. |