Abstract: The present invention relates to a silver braze alloy having improved wetting properties. The silver braze alloy consists essentially of from about 52.25 wt % to about 57.0 wt % silver, from about 38.95 to about 43.0 wt % copper, from about 0.5 wt % to about 5.5 wt %, preferably from about 1.0 wt % to about 5.5 wt %, manganese, and up to about 2.5 wt %, preferably from about 1.5 wt % to about 2.5 wt %, nickel. The alloy further may contain 0.15 wt % total of other trace elements. |
Filed: 12/29/2000 |
Application Number: 9/752000 |
This invention was made with Government support under Contract No. DE-NA0003525 awarded by the United States Department of Energy/National Nuclear Security Administration. The Government has certain rights in the invention. |
Attribution for Derwent World Patents Index Records published on Sandia ® echo date('Y'); ?> Clarivate. All rights reserved. Republication or redistribution of Clarivate content, including by framing or similar means, is prohibited without the prior written consent of Clarivate. Clarivate and its logo, as well as all other trademarks used herein are trademarks of their respective owners and used under license. |